Nanoindentation Tip mechanics ascribing bluntness during fracture of thin coatings
- A S Bhattacharyya
![](https://d197for5662m48.cloudfront.net/assets/icons/omniauth/orcid-ca37582cd91a671ed5cec57770e0e96c01b4b79b8b5b75d8598fc1ddac18c974.svg)
A S Bhattacharyya
![](https://d197for5662m48.cloudfront.net/assets/icons/omniauth/orcid-ca37582cd91a671ed5cec57770e0e96c01b4b79b8b5b75d8598fc1ddac18c974.svg)
Department of Metallurgical and Materials Engineering, Central University of Jharkhand
Corresponding Author:[email protected]
Author ProfileAbstract
Nanoindentation is used for the determination of mechanical properties of thin-coatings comprising a mixture of hard phases. The load-depth plots represent minor fracture (energy ~ pJ) taken place due to assorted crystallization on the surface. The tip movement during the fracture is influenced by strain hardening due to brittle to ductile transformation and the amount of tip-bluntness as evident from the fractorial normal stiffness.